Maraging 350





Lork Group high-quality Maraging 350 has excellent mechanical properties, workability and heat treatment characteristics. Used for missile and rocket motor cases, landing and takeoff gear components, high performance shafting, gears and fasteners.
Lork Group high-quality Maraging 350/ UNS S35000/ is a nickel-maraging alloy that is relatively soft, but extremely tough. Maraging 350 can also be readily machined and formed to your specifications. In addition, the aging process of Maraging steel raises the hardness to a level sufficient for many tooling applications.
Maraging 350 has excellent mechanical properties, workability and heat treatment characteristics. Maraging 350 is used for missile and rocket motor cases, landing and takeoff gear components, high performance shafting, gears and fasteners.
Bars, Forgings, Mechanical tubing and flash welded rings: AMS 6515
Maraging 350 Chemical Composition
|
|
|
|
|
63 |
|
|
|
|
|
12 |
|
|
4.8 |
|
|
1.4 |
|
|
0.1 |
|
|
<= 0.10 |
|
|
<= 0.10 |
|
C |
<= 0.030 |
|
S |
<= 0.010 |
|
P |
<= 0.010 |
|
|
0.01 |
|
B |
0.003 |
Maraging 350 Property
|
|
0.2 % Yield Strength ksi |
|
Elongation in 4D(%) |
|
Maraging 350 |
330 |
350 |
8 |
Maraging 350 Application